Hi Dan,
We have the LPKF routing system as well, and we use T-Tech system for
plating and lamination. It use conductive ink (to replace the electroless
plating) for hole plating to connect all the layers, and copper plate on
top. The conductive ink process is so unreliable. Every step has to be
perfect to get a reasonable result, but you can't tell until you get the
board done and test it. What do you use for plating, the Kepro system? To
me, holes have to go through the proper plating process. Using conductive
ink for multi-layer is just not right.
I appreciate your response. Thanks.
Patrick
"Dan R. Johnson" <[log in to unmask]>@IPC.ORG> on 10/28/2002 09:15:43 AM
Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond
to "Dan R. Johnson" <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
To: [log in to unmask]
cc:
Subject: Re: [TN] PCB Prototyping
Patrick,
I was disappointed that this post didn't get more replies. We had a similar
situation so I was interested in the opinions of the experts. Although we
use the LPKF system I think that our solution might help. We played around
with trying to replenish the plating bath, eventually we completely
replaced
it and that solved the problem. It may not be the plating bath in your
case.
What we actually learned was that we needed to know more about the
chemistry
involved.
I would suggest that you figure out how to evaluate each solution and
maintain it. The system vendor may be less than candid since they are
selling you the consumables so it might take some home work. Try to find
out
who actually manufactures the chemicals you use and contact them direct.
They usually don't sell in the small quantities that you would use but they
may be willing to help with analysis and or advice.
Perhaps some of the PCB experts on Tech net could suggest reference
material
that could help?
Hoping you experience is less painful than ours,
Dan
----- Original Message -----
From: <[log in to unmask]>
To: <[log in to unmask]>
Sent: Thursday, October 24, 2002 12:29 PM
Subject: [TN] PCB Prototyping
> Hi TechNetters,
>
> My company have set up a PCB prototyping Lab, with a Rapid PCB
Prototyping
> machine. It works good on routing and laminating, but when it comes to
through
> hole plating, it's a nightmare. The Quick Plate System just couldn't do a
> reasonable plating job. I doubt if the process it uses to replace the
> electroless plating really works. I would appreciate any suggestions to
improve
> it, or what can we get to replace this Quick Plat System.
>
> Thanks,
>
> Patrick
> This e-mail may contain SEL confidential information. The opinions
expressed
> are not necessarily those of SEL. Any unauthorized disclosure,
distribution or
> other use is prohibited. If you received this e-mail in error, please
notify
> the sender, permanently delete it, and destroy any printout. Thank you.
>
> ---------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for
additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
> -----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|