IPC-HDBK-001 5.1.2
Brass is an alloy consisting mainly of copper and zinc. Without a
barrier layer of copper or nickel over the brass, the zinc will dissolve
into the molten solder during soldering, Zinc contamination of the
solder joint is evident by a rough, grainy, frosty, porous surface with
a high dendritic structure. Also, solder wetting to the terminal would
be inhibited.
Wish I knew more, perhaps Dhillman would find time to comment?
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Phil Nutting
> Sent: Thursday, October 03, 2002 3:23 PM
> To: [log in to unmask]
> Subject: [TN] soldering brass to copper
>
>
> I vaguely remember something about soldering brass in some
> recent posts. We are looking at some cooling parts that may
> require soldering brass to copper. My experience says that
> this is a non-problem. The posts that I remember said
> something about tin and crystallization. Am I mixing two
> different thoughts here?
>
> Phil Nutting
> Manufacturing Engineer
> Kaiser Systems, Inc.
> voice: 978-922-9300
> e-mail: [log in to unmask]
>
> --------------------------------------------------------------
> -------------------
> Technet Mail List provided as a free service by IPC using
> LISTSERV 1.8e To unsubscribe, send a message to
> [log in to unmask] with following text in the BODY (NOT the
> subject field): SIGNOFF Technet To temporarily halt or
> (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE
> mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest Search the archives of
> previous posts at: http://listserv.ipc.org/archives Please
> visit IPC web site http://www.ipc.org/html/forum.htm for
> additional information, or contact Keach Sasamori at
> [log in to unmask] or 847-509-9700 ext.5315
> --------------------------------------------------------------
> -------------------
>
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|