I managed and later owned a janitorial service ( and sold the chemicals )long ago. Concrete. Tiles come loose, carpet fibers break off and the carpet can get hard to maintain in a working environment. If you use one of the ESD waxes be sure to seal the floor with the appropriate sealer first. 2 year wearability? Not likeley unless they mean with a regular touch up treatment. Proper upkeep is important, mainly for looks as the bare concrete should provide adequate ground. Also all of the ESD "waxes" I am familiar with are acrylic based and not very chemical resistant. Alkalis and most solvents will attack the finish. In fact the stripper for this type of finish is essentialy sodium hydroxide and an emulsifier.
Another option is conductive floor paint. This also requires some upkeep. ESD wax will keep it looking good. The color options are limited. The paint was only available in beige, grey and black when I sold the stuff. Reccomend the grey. Black shows scuffs and dirt, beige is just ugly. As for different brands feel free to contact me direct.
Charles Caswell
[log in to unmask]
-----Original Message-----
From: Phil Nutting [mailto:[log in to unmask]]
Sent: Thursday, October 31, 2002 10:17 AM
To: [log in to unmask]
Subject: [TN] ESD floor wax
Good morning,
We are looking at some new assembly space an we have an opportunity to make the floor whatever we want. Three options, ESD tiles, ESD carpet or ESD wax. Regarding the ESD wax, does anyone have opinions about 4500 Staticide Gold or 4600 Staticide Ultra available from Techni-Tool? Is the 24 month "wearability" a real number?
If you prefer, offline comments gladly accepted.
Thanks in advance,
Phil Nutting
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|