Jonathan;
Are you sure you don't have an intermetallic layer or is it that you just can't sdee it on an optical micrograph of a cross section. One problem you run into when you use Sn95Sb5 and you try to compare it to Sn8Pb88Ag2 or even Sn63Pb37 is that there is very little optical contract without the lead (Pb) being present. You can usually detect the difference between copper-tin intermetallic and the bulk SnSb solder using SEM/EDX if you have good cross sections and if you have really good cross sections you can also also see the difference on optical micrographs.
Regards,
George
George M. Wenger (908)-546-4531
Reliability Engineer
RF Power Amplifier Group
Andrew Corporation, 40 Technology Drive, Warren, NJ 07059
[log in to unmask]
-----Original Message-----
From: [log in to unmask]
[mailto:[log in to unmask]]
Sent: Monday, October 28, 2002 4:36 AM
To: [log in to unmask]
Subject: [TN] Lead -Antimony experience
Hello Techies:
Does anyone of you have a weird experiences on Sn-Sb alloy for
soldering? (Lead free)?
In my case i have a separation between a Cu surface and the SnSb (95/5)
after HTSL test at the intermetallic layer, in which i can't find any from
88Pb8Sn2Ag solder paste.
Is Antimony can promote kirkendall voiding during the Sn and Cu bonding?
If somebody uses 95/5 (Sn/Sb) for soldering, what are the usual problems,
your were encountering?
Does Sb affects Sn diffusion on Cu metal? If yes what would be the optimum
alloy composition.
Appreciate your help
regards
Jonathan
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
------------------------------------------------------------------------------------------------
This message is for the designated recipient only and may
contain privileged, proprietary, or otherwise private information.
If you have received it in error, please notify the sender
immediately and delete the original. Any unauthorized use of
this email is prohibited.
------------------------------------------------------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|