Susan,
I don't believe that your question can be answered without more information.
The print and specifications need to be considered, too. One scenario that
comes to mind is that this is a design where the dielectric thickness and
line widths are specified. The nominal dimension would be used to indicate
the designer's calculated dielectric. The thickness is not critical and is
used to cover the accumulated tolerances. In this case, if all of the
specified dielectrics and the overall thickness are in tolerance and the
.0035 thickness meets any specified minimum dielectric specifications, I
would judge that the product meets specification.
However, since I don't have the documents available for review, this is all
hypothetical.
Don Vischulis
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of [log in to unmask]
Sent: Thursday, October 10, 2002 10:08 PM
To: [log in to unmask]
Subject: [TN] nominal
OK, so I now have several opinions - completely opposite of one another.
So here is an example:
Drawing lists 0.009" dielectric thickness as nominal
Actual value is 0.0035"
Does that meet the designer's needs?
Susan
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|