There are only two sources I know of for laminate this size - Nelco (Dielektra) in Germany who have a contilam press, and can do any length you want, and Polyclad in Sweden who have a press that can make this size sheet. There is a problem that people cannot cut this size sheet on a guillotine, as the blade width is 56" !
I am currently at the EIPC show in Germany, and Nelco have a laminate in their suite that I believe is 25feet long (but only 24" wide) but its rather heavy to lift !
Dougal Stewart
> from: SDC's Tech Net <[log in to unmask]>
> date: Tue, 08 Oct 2002 23:16:52
> to: [log in to unmask]
> subject: Re: [TN] Looking for Extra Large Panels(size:48"X96") of FR-4 Material.
>
> Hello! everybody,
> I am in need of extra large panel size.I am looking for 48"X96" FR-4
> material.0.014"thick core with 1/2 oz copper on both side.Any help on this
> would be appriciated.
>
> Thank you.
> Kris Vasoya
> VP of Operations.
> Thermal Works
> ph:714-540-8454 Ext:202
> fax:714-540-1299
> e-mail: [log in to unmask]
> www.thermalworks.com
>
> ---------------------------------------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> ---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|