Probably nothing. Several years ago I was tasked with finding what the " contamination" was that was causing some " dewetting" both on solder and conformal coat. I purposely applied differnt possible contminants to marked sections of a large board. The area sprayed with WD-40 soldered fine with RMA flux. This was on HASL boards so I doubt you will have much trouble with gold. A run through whatever cleaning process you use should be sufficient
Charles Caswell
Process Lead, PCB
Frontier Electronic Systems
-----Original Message-----
From: Barbara Burcham [mailto:[log in to unmask]]
Sent: Thursday, September 19, 2002 11:19 AM
To: [log in to unmask]
Subject: [TN] How to use gold finished boards that have been handled?
Technetters,
We have a gold finish over nickel that we have passed around and drooled over. Now, we want to clean it up and assy. it.
What do we need to do to remove hand oils from the metal so that it will solder?
Barbara J. Burcham, C.I.D.
Sr. PCB Designer
Fairfield Industries
Sugar Land, TX 77478
281-275-7687 Work
281-275-7550 Fax
[log in to unmask]
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|