I don't think that intermittent failures could be detected by X-ray, because
cracks are very hard to see with this method. If the failure is not related
to cracks you have a chance.
Gaby
----- Original Message -----
From: "Peter Lee" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Wednesday, September 18, 2002 2:23 AM
Subject: [TN] BGA failure and Rework
> Technet,
>
> If I may continue my question on BGA rework process:
>
> Recently we have seen intermitted failures from a few BGA assemblies.
> After removing the suspicious BGA on the rework station we noticed
> dewetting on a majority number of pads of the removed BGA. The solder
> ball residues were mostly attaching to the board.
>
> Has anyone seen this before? How likely can this be caused by a
> non-optimum rework removal profile Is baking of the board normal prior
> to rework (removal/re-placement)?
>
> We are tackling this issue from the part supplier side and looking at
> performing destructive X-ray analysis. Can someone give me an idea of
> what the ball attachment process is on the BGA?
>
> Rgds,
> Peter
>
> --------------------------------------------------------------------------
-------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
> --------------------------------------------------------------------------
-------
>
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|