Try to contact Indium Corporation of America.
We were using type for our Flip Chip. I guess they
have type 6 on their standard alloys.
regards
sahmad
<[log in to unmask] To: [log in to unmask]
M> cc:
Sent by: TechNet Subject: [TN] solder paste below Type 5
<[log in to unmask]>
09/13/02 06:30 AM
Please respond to
"TechNet E-Mail
Forum."; Please
respond to sahmad
Is there a supplier for Type 6 or Type 7 solder paste?
Syed Sajid Ahmad
Advanced Packaging Technology/F4
Mail Stop 718
Micron Technology, 8000 S. Federal Way, Boise ID 83716-9632
(208)368-3359 Fax (208)363-2994
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------