Hello Gary
Looks like McMaster-Carr might have what you need. Throat is 1.25 deep and
jaw is 1 inch wide. Pressure is screw adjustable from 1 to 50 lbs. stock#
51115A14 @ $2.56 www.mcmaster.com
John Thorup
> -----Original Message-----
> From: Gary Camac [SMTP:[log in to unmask]]
> Sent: Tuesday, September 03, 2002 11:53 AM
> To: [log in to unmask]
> Subject: [TN] Spring clamp
>
> Afternoon everyone,
>
> I trying to locate a spring clamp. Throat depth .7" - 1.2". Clamping
> pressure - 4 lb.
> +/- 1 lb. Width - .5" - 1". Actually a spring type clothes pin almost
> would fit the
> bill, if only they would deliver the clamping pressure. I would like to
> see the manager's
> face at Walmart, when I ask to test his clothes pins with my force gauge.
>
> Thanks in advance,
> Gary Camac
>
> --------------------------------------------------------------------------
> -------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
> ext.5315
> --------------------------------------------------------------------------
> -------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|