Now that is interesting and very valuable information. I will follow this
very closely even from "outside" the round robin and other reliability
testing.
Thanks a bunch Werner,
Earl
----- Original Message -----
From: "Werner Engelmaier" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Friday, September 06, 2002 1:17 PM
Subject: Re: [TN] IPC-TM-650-2.6.8, Thermal stress, Plated Through Holes
> Hi Earl,
> ILS was previously referred to 'post-separation.'
> Actually, the forces are not exerted diagonally to the trace/pad to
conductor
> interface, but radially relative to the PTH barrel. This is the result of
the
> PTH barrel experiencing the same compression deformation as a submarine on
> diving; except, of course, that a submarine has its reinforcement ribs on
the
> inside and the PTH barrel on the outside [that's the functional and
> non-functional lands]. The traces resist the compressive movement of the
> barrel and failure can occur at the weakest of 3 links [ plating/flash
> interface, flash/foil interface, foil]. When the compressive deformation
is
> plastic for the copper barrel, hole separation occurs as the resin returns
to
> its former position on cooling.
>
> Werner
>
> --------------------------------------------------------------------------
-------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
> --------------------------------------------------------------------------
-------
>
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|