*Caution* use a "Pink Pearl" type eraser, the type used for ink will remove
the gold plate. (He remarked sheepishly.) Yes, this is the voice of
experience. I learned this lesson in the eighties building/repairing traffic
controller modules.
Dan
---------------------------------------------------------------------------------