I like that post. Actally found with SRT nozzles the specified .110" spacing
all around the device to nozzle clearance was/is very important. Beyond
that, for some BGA types as supers, the nozzle to board clearance needed to
be about 80 thou or so and with paste flux, this worked very well.
MoonMan
---------------------------------------------------------------------------------