Mr. MoonMan,
I appreciate all the input from the community on my inquiry.
I will clarify my initial request.
During the INSPECTION PROCESS is the inspector restrained from
using other MAGNIFICATION than those described in IPC-A-610C Table 1-2
Inspection Magnification.
Need additional description for Land Width, CONDUCTOR TRACES ????,
or LAND DIAMETERS, ANNULAR PADS ??,
Is the INSPECTOR allowed any means of MAGNIFICATION to identify a
potential defect.
Victor,
-----Original Message-----
From: Earl Moon [mailto:[log in to unmask]]
Sent: Friday, September 06, 2002 2:01 PM
To: [log in to unmask]
Subject: Re: [TN] Difference in TERMINOLOGY
Victor,
IPC-6012A clearly is, as its title denotes, a qualification and performance
specification for rigid printed boards. Any inspection, no matter where
performed, is done in accordance with IPC-A-600F.
Earl
----- Original Message -----
From: "Victor Hernandez" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Friday, September 06, 2002 11:56 AM
Subject: [TN] Difference in TERMINOLOGY
> Fellow TechNetters,
>
> Is there a difference in TERMINOLOGY are is INSPECTION & RECEIVING the
> same as would be a QUALIFICATION of product.
> Any HELP with literature and/or industry definition of the two arenas.
> This is a serious subject. I understand that QUALIFICATION
> would require all means available to determine probable material failure
and
> use of material selection.
>
> Victor G. Hernandez
> Component/Material Failure Analysis Eng.
> PS4-1, Rm. 132
> Ofc: 512-725-3471
> Pgr: 512-907-0005
>
> --------------------------------------------------------------------------
-------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
> --------------------------------------------------------------------------
-------
>
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|