Try J-STD-001C Table 5-1 for contaminant limits.
Rick
-----Original Message-----
From: McCall,Doug [mailto:[log in to unmask]]
Sent: Monday, September 23, 2002 4:16 AM
To: [log in to unmask]
Subject: [TN] Wave solder bath analysis
Techies,
I am interested in finding out what the solder analysis figures
should be from the sample taken from the flow solder bath sample.
Percentages of the following elements would be useful: -
Tin, lead, antimony, copper, zinc, iron, nickel, bismuth, cadmium,
Silver, gold, arsenic, aluminium etc.
We are using 63 / 37 bar solder into the machine.
Also any mil-spec equivalents would be useful.
Thanks in anticipation,
Regards,
Doug McCall
PCB Manufacturing Engineer - Eastbourne
BOC EDWARDS
Marshall Road,
Eastbourne,
East Sussex,
BN22 9BA UK
Tel: +44 (0) 1323 501 147
Fax +44 (0) 1323 509 824
mailto [log in to unmask]
BOC Edwards is a part of BOC Limited
Registered Office: Chertsey Road, Windlesham, Surrey GU20 6HJ
Number 337663-English Register
Ultimate holding company: The BOC Group plc
_____________________________________________________________________
This e-mail has been scanned for viruses by the WorldCom Internet Managed Scanning Service - powered by MessageLabs. For further information visit http://www.worldcom.com
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|