We currently use a no-clean process {no wash process} with our assemblies and have
had the following issues to contend with.
1} Unactivated no-clean flux leaves a white residue on the board. Although this is non-
corrosive it is unsightly to the customer. We have been using a hot-air rework station to
remove this residue by activating the flux till it disapperars.
2} We did try at one point to try and clean the boards with a cleaner "prozone" but this
is not recommended. The reaction between the flux and the prozone caused the areas
applied to become hydoscopic and absorb moisture. The boards then started to "grow"
a white residue almost powder like growth.
3} On hand soldering of parts after wave solder, we used to use the same flux that was
in the solder bath, but although the board looks clean immediately after the sodlering
process, if it is left for approx 24hours then this unactivated flux residue appears. We
combat this by only using a rework gel flux for apply to the board before hand soldering.
Hope this helps...
On 19 Sep 2002 at 23:10, Peter Lee wrote:
Date sent: Thu, 19 Sep 2002 23:10:26 -0700
Send reply to: "TechNet E-Mail Forum." <[log in to unmask]>,
Peter Lee <[log in to unmask]>
From: Peter Lee <[log in to unmask]>
Subject: [TN] Noclean Wave soldering
To: [log in to unmask]
> Technet,
>
> Is anyone currently adopting a no clean flux/ no post wash with their
> Wave soldering process? We had a few wave soldered products requiring
> post hand soldering due to non-washable components (filters,
> transformers etc.)
>
> In particular, I like to know what areas of concern you run into (eg.
> Remaining Flux residues, conformal coating) and your feedback on the
> overall cleanliness of the boards.
>
>
> Rgds,
> Peter
>
> ---------------------------------------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> ---------------------------------------------------------------------------------
Best Regards
Gordon McAlpine
Test Engineering Manager
Telspec Scotland Ltd
Tel :- 01738 494500
DDI :- 01738 494506
Fax :- 01738-630012
E-Mail :- [log in to unmask]
================================================
DISCLAIMER
This message is intended only for the use of the individual(s) or entity
named above.
It may contain information which is privileged or confidential.
If you are not the intended recipient, please return it to the sender
as soon as possible and be aware that any disclosure, copying,
distribution or use of the contents is prohibited.
The views expressed in this communication may not necessarily be the
views
held by the Company.
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|