Tom,
(1) Over heat the polyimide board will result dis-coloration and
brittlement.
(2) yes, not all the polyimide are made equal.
(3) TMA is more sensitive than DSC for the Tg measurement. Usually, a bit
lower Tg observed when use TMA technique compare to DSC.
my 2 cents.
jk
>-----Original Message-----
>From: TechNet [mailto:[log in to unmask]]On Behalf Of Tom Waznis
>Sent: Wednesday, September 18, 2002 10:37 PM
>To: [log in to unmask]
>Subject: Re: [TN] Poyimide cure
>
>
>Pretty hard to overcure Polyimide with that high a Tg. Too long at
>high temperatures can make the material more brittle.
>Hope your using one with Tg of 240-260 (similar to the old 601, 601A
>resin that is no longer available). Some of the new ones have
>significantly lower Tg.
>
>
>Since Polyimide resin systems now vary (no more 601A) from supplier to
>supplier The supplier should be consulted. In general the heat rises
>are similar to FR4s but the material is usually significantly thicker
>than FR4 while it is flowing. Higher pressures than FR4 are typical
>but not really needed for all builds; depends how much you are
>actually filling.
>
>Tg can be done anytime. DSC or TMA is ok; I prefer DSC.
>At lest one formula requires two cure times / temperatures and time at
>the higher temp. does NOT count for the first required time at the
>lower temp.
>
>[log in to unmask] wrote:
>> Technetters:
>> I'm looking for information on the best way to confirm cure on a
>> polyimide board. The particular part is a sequential lamination
>> structure.
>> My questions include:
>> 1. Is the best time to confirm cure of polyimide immediately after
>> final lamination?
>> 2. Do the polymers created require a specific cure test, e.g. is TMA
>> best, DSC, or other method?
>>
>> Also, can overcure be a problem with Polyimide?
>>
>> And, does this material offer special challenges with respect to gel
>> time, resin flow, etc?
>>
>> I've already heard differences of opinions, and am looking forward to
>> more avenues of knowledge from Polyimide experienced folks.
>>
>> Mark Julstrom
>>
>Multek-------------------------------------------------------------
>--------------------
>> Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
>> To unsubscribe, send a message to [log in to unmask] with following text
>> in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt
>> or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET
>> Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
>> posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
>> archives of previous posts at: http://listserv.ipc.org/archives Please
>> visit IPC web site http://www.ipc.org/html/forum.htm for additional
>> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
>> ext.5315
>>
>-------------------------------------------------------------------
>--------------
>>
>
>-------------------------------------------------------------------
>--------------
>Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail
>to [log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
>information, or contact Keach Sasamori at [log in to unmask] or
>847-509-9700 ext.5315
>-------------------------------------------------------------------
>--------------
>
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|