We have thick boards plated up and don't have lifted lands. It depends on the material and design. I would like the paragraph to stay the way it is. If someone is okay with lifted pads and it is a design issue it can go on their drawing.
Rene
-----Original Message-----
From: Benny Nilsson (EAB) [mailto:[log in to unmask]]
Sent: Monday, September 30, 2002 12:23 AM
To: [log in to unmask]
Subject: Re: [IPC-600-6012] Proposed Change to Acceptance Criteria for
Lif ted Lands
Hello John. Does it realy need to be stated "agreed upon between user and supplier"? In my opinion "agreed upon...." is a part of "Approved PB Procurement Documentation" see Section 3.5 in -6011.
Begards Benny
-----Original Message-----
From: John Perry [mailto:[log in to unmask]]
Sent: den 27 september 2002 23:40
To: [log in to unmask]
Subject: [IPC-600-6012] Proposed Change to Acceptance Criteria for
Lifted Lands
Colleagues,
IPC would like a task group disposition on the following comment for the IPC-6012 B Revision effort.
Ted Edwards of Dynaco Corporation has proposed rebuilding paragraph 3.3.4 in the IPC-6012B 2nd Working Draft relative to allowances for Lifted Lands to read:
When visually examined in accordance with 3.3, the finished board shall not exhibit any lifted lands unless agreed upon between user and supplier.
Reason for Recommended Change: On thick boards with thick plating requirements, if a HASL finished is used there almost always exists lifted lands and this statement would mean that they would all have to be scrapped.
Your reply is appreciated.
Regards,
John Perry