Subject: | |
From: | |
Reply To: | TechNet E-Mail Forum. |
Date: | Fri, 16 Aug 2002 09:37:25 -0700 |
Content-Type: | text/plain |
Parts/Attachments: |
|
|
Rudy,
Production person here. I ran the then Dexter FST for about two years and
thicknesses of 30 microinches were steadily maintained. When a "decant" of
the bath was performed we had alot of readings in the 40 range for a couple
of weeks but then would taper back off into the 30's. I also evaluated the
then McGean Rohco immersion tin also which seem to perform much like the
Dexter.
Tony Steinke
AIT-Atlanta Inc.
----- Original Message -----
From: "Rudy Sedlak" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Thursday, August 15, 2002 3:56 PM
Subject: [TN] Immersion Tin Thickness
> There are some numbers being thrown around for immersion Tin Thickness
that
> are a little unrealistic.
>
> Getting 40+ microinches (1+ micron) is pretty difficult, to impossible on
a
> production basis. It can be done in a lab, with a freshly made up bath,
but
> I have never seen even 50 microinches ever, and this is with any immersion
> Tin process.
>
> Is anyone even maintaining 40 microinches in production?
>
> I suspect that you have to run your process pretty carefully to maintain
30+
> as the bath gets old.
>
> Will production people comment please?
>
> Rudy Sedlak
> RD Chemical Company
>
> --------------------------------------------------------------------------
-------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
> --------------------------------------------------------------------------
-------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|