TECHNET Archives

August 2002

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-type:
text/plain; charset=us-ascii
Sender:
Subject:
From:
Date:
Wed, 7 Aug 2002 08:27:20 +0800
MIME-Version:
1.0
X-To:
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Parts/Attachments:
text/plain (84 lines)
Hi, Yuan,

There are some postings in the TechNet archives about 'Fatigue Resistant
Solders'. These are like normal solders, but have dopants added that make
their grain structure much finer. They have been developed specifically for
BGA and CLCC applications where solder joint inflexibility has caused creep
fatigue failures with substrate materials that have a significantly
different CTE. Look up "fatigue resistant solder" on the Net, and you'll
find what I found, which isn't a lot, but it is growing as research is
carried out and completed. The potential downside to FRS's is that they
have a lower melting point than 'normal' solders. If your assembly is
manufactured with an FRS and it subsequently goes through a wave soldering
process that uses normal solder, the chances are that your components will
move or even fall off. So be careful! Using a FRS may reduce the thermal
stresses on you BGA joints, or permit better solder joints at the lower
temperatures that BGA's seem to reach in the Convection Reflow pre-heat
stages, but as BGA balls are of normal eutectic solder, these may not be
compatible with FRS's - the FRS will melt and reflow, but the BGA balls may
only partially flow, and this could give you more trouble than started
with.

Take it carefully and do a full evaluation of whatever options you go for.

Peter



Yuan Li <[log in to unmask]>     06/08/2002 12:10 AM
Sent by: TechNet <[log in to unmask]>

Please respond to "TechNet E-Mail Forum."; Please respond to Yuan Li

              To:  [log in to unmask]
              cc:  (bcc: DUNCAN Peter/Asst Prin Engr/ST Aero/ST Group)
              Subject: [TN] Solder creeping








Hi,
Wondering anyone knows what additives can be added into the eutectic solder
system to slow down the creeping effect ?
Thx,
Yuan

---------------------------------------------------------------------------------

Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
---------------------------------------------------------------------------------





[This e-mail is confidential and may also be privileged. If you are not the
intended recipient, please delete it and notify us immediately; you should
not copy or use it for any purpose, nor disclose its contents to any other
person. Thank you.]

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2