talk to these guys about soldering silver.... good luck (poor wetting is
possibly blame...).
http://www.kester.com/faq_solder_alloys.html
jk
>-----Original Message-----
>From: TechNet [mailto:[log in to unmask]]On Behalf Of Jack C. Olson
>Sent: Friday, August 02, 2002 2:23 PM
>To: [log in to unmask]
>Subject: [TN] ASSY: Immersion Silver vs. Tin
>
>
>Greetings,
>
>A situation has come up that is beyond my experience.
>
>We sent some Immersion Silver boards to an assembly
>vendor and recieved an email saying:
>
>"We are progressing on your boards. The bad news is
>that the white tin flash used on the pads is awful.
>The solder is reflowing irregularly, if at all.
>We suspect that we'll have to touch every joint on
>every part to make a good connection."
>
>So my question to the group is:
>Is there a difference from an assembly process point of view
>between tin and silver?
>
>I'm hoping the root problem is related to their assumption
>that our silver boards were tin, but I don't know enough
>about it.
>
>Thanks in advance for any clues....
>
>Jack
>
>-------------------------------------------------------------------
>--------------
>Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail
>to [log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
>information, or contact Keach Sasamori at [log in to unmask] or
>847-509-9700 ext.5315
>-------------------------------------------------------------------
>--------------
>
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|