Not wax, only Dow Corning's silicone 3140 some years ago. This has
"self-healing" properties as well and allows the use of test probes (in
moderation) without jeopardising the integrity of the coating. It can be
sprayed, dipped or brushed on. Board cleanliness is important to adhesion.
Peter
David Hannick <[log in to unmask]> 14/08/2002 06:57 PM
Sent by: TechNet <[log in to unmask]>
Please respond to "TechNet E-Mail Forum."; Please respond to David Hannick
To: [log in to unmask]
cc: (bcc: DUNCAN Peter/Asst Prin Engr/ST Aero/ST Group)
Subject: [TN] wax conformal coatings
hi.
Has anyone experienced or heard of using wax as a type of cheap conformal
coating. Our company is looking at conformal coatings at the moment but
equipment costs are high, our product has low margins and our manufacturing
process would have to change from a cell / line (one piece flow) set up to
a
batch setup.
We were thinking that we may just have to coat one side of the boards only
and so wax could be applied using wave soldering type equipment.
Our main problem with using regular conformal coatings is that our final
functional tests are carried out via test pads while the PCBs are in their
plastic enclosures. Wax would allow us to continue doing this as the test
pins could pierce through the wax to contact the test pads and afterwards
these pin holes would be minimal as wax has a small degree of reflow /
creep. Otherwise we would have to selectivily spray the conformal coatings,
missing the test pads but leaving them more vunerable to damage / corrosion
while is service.
Has anyone any experience of wax coating PCBs.
Best regards
David Hannick
Ei Electronics
Shannon
Ireland.
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
---------------------------------------------------------------------------------
[This e-mail is confidential and may also be privileged. If you are not the
intended recipient, please delete it and notify us immediately; you should
not copy or use it for any purpose, nor disclose its contents to any other
person. Thank you.]
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|