TECHNET Archives

August 2002

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Subject:
From:
Earl Moon <[log in to unmask]>
Date:
Fri, 9 Aug 2002 11:18:43 -0500
X-To:
Bill Page <[log in to unmask]>
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Earl Moon <[log in to unmask]>
Parts/Attachments:
text/plain (27 lines)
Oldy but goody, Bill.

I, and who am I really, specify in my master drawing notes vias shall be
tented under BGA devices - especially under .8mm CSP types just to avoid
going to micro vias and all the rest going with it.

I am concerned about your concerns concerning entrapped contamination (I do
love aliteration) in production boards. However, this concern apparently is
not being concerned by industry or is it lately in light of all this
cleanliness stuff?

I still want to know if we need to go back to two ply minimum dielectric
materials. Seems like this CAF stuff is headed back that way.

MoonMan

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2