Chuck: The Shipley Mechanical Bulge Tester (love that name) is typically
used to check the tensile strength of electroplated copper. It was a rod
that deflects the copper plate. They marketed in the late 80's early 90's.
Don't know if it's still available.
If Shipley doesn't carry it anymore, might be available on the used
equipment market.
Regards
Michael Barmuta
Staff Engineer
Fluke Corp.
Everett WA
425-446-6076
-----Original Message-----
From: Brummer Chuck [mailto:[log in to unmask]]
Sent: Wednesday, August 28, 2002 10:14 AM
To: [log in to unmask]
Subject: [TN] Shipley Bulge Tester
Hi,
Does anyone know anything about the Shipley SE 800 Mechanical Bulge Tester?
I need to find one to test, rent or whatever. The Shipley web site was not
very helpful.
We have a procedure that calls for this equipment.
Thanks in advance
Chuck Brummer
Acuson (A Siemens Co.)
818.734.4930
----------------------------------------------------------------------------
----- Technet Mail List provided as a free service by IPC using LISTSERV
1.8e To unsubscribe, send a message to [log in to unmask] with following text
in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/html/forum.htm for additional information, or
contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|