Rick: Teflon will soften when heated. It is also not as rigid as standard
FR4 material at room temp. If it is all Teflon construction(no external
layers of a more rigid material)you may require fixturing with bottom
supports or a backup board. This is especially true during reflow where it
can sag.
The other issue is if it is a Teflon MLB the internal bonding film is
thermally sensitive and could delaminate if heated or stressed excessively.
Regards
Michael Barmuta
Staff Engineer
Fluke Corp.
Everett WA
425-446-6076
-----Original Message-----
From: Rick Thompson [mailto:[log in to unmask]]
Sent: Wednesday, August 14, 2002 7:37 AM
To: [log in to unmask]
Subject: [TN] Teflon PCB Processing?
We have a customer using a Teflon laminate in one of their designs. Can
anyone tell me if there are things we should be aware of when processing
these boards through standard surface mount processes (print, place,
reflow, clean, etc) that are different than say standard FR4 type
materials?
Thanks,
Rick Thompson
Ventura Electronics Assembly
2655 Park Center Dr.
Simi Valley, CA 93065
+1 (805) 584-9858 x-304 voice
+1 (805) 584-1529 fax
[log in to unmask]
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|