Ya know, Sona Tubes at Home Depot may work.
Bottom line is you have versatility for completing the task.
----- Original Message -----
From: James TerVeen <[log in to unmask]>
To: <[log in to unmask]>
Sent: Friday, August 23, 2002 1:28 PM
Subject: [TN] NTC Re: [TN] Emptying wave solder pot
> Steve, maybe you can call "charmin" and see if they can send you a few
> hundred of the small size holders or maybe ask everyone in the plant to
> bring in a couple over the next few weeks as they become empty from home
> and you may have enough. Seriously though in a past life we used small
> bread loaf pans that were coated to pour it into and then as they cooled
we
> would reuse them. They stack nice and if you are going to use them again
> then they are small enough to fit back into the pot.
>
> Maybe you could call Bounty paper towel and get the larger size. you
> need a little fun every now and then.
>
>
>
>
> Steve Gregory
> <[log in to unmask] To: [log in to unmask]
> M> cc:
> Sent by: TechNet Subject: [TN] Emptying
wave solder pot
> <[log in to unmask]>
>
>
> 08/23/02 08:46 AM
> Please respond to
> "TechNet E-Mail
> Forum."; Please
> respond to
> SteveZeva
>
>
>
>
>
>
> Hi All!
>
> In a couple of weeks, I'm going to have to empty the wave solder pot on
our
> Treiber.
>
> In the past, I remember round cardboard containers being used to put the
> solder in after ladling it from the pot. Does anybody know where I can get
> those?
>
> Thanks!
>
> -Steve Gregory-
> --------------------------------------------------------------------------
-------
>
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To
> unsubscribe, send a message to [log in to unmask] with following text in the
> BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
> (re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet
> NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
> e-mail to [log in to unmask]: SET Technet Digest Search the archives of
> previous posts at: http://listserv.ipc.org/archives Please visit IPC web
> site http://www.ipc.org/html/forum.htm for additional information, or
> contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> --------------------------------------------------------------------------
-------
>
> --------------------------------------------------------------------------
-------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
> --------------------------------------------------------------------------
-------
>
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|