Victor,
generally speaking, Au/PdNi/Ni is a better contact finish than Au/Ni. This
is mainly due to the increased hardness and decreased porosity of
Au/PdNi/Ni compared to Au/Ni. The downside of PdNi finish is the Pd price,
which has been high and volatile until few months ago. I will e-mail you
some papers directly to your e-mail address (don't want to overload this
mailing list).
Chen
Chen Xu
Enthone, Inc.
CRL
600 Route 440
Jersey City, NJ07304
Tel. (201)-4346778 ext. 2042 (o)
ext. 2051 (lab)
Fax. (201)-4342529
[log in to unmask]
Victor Hernandez
<Victor_G_Hernandez To: [log in to unmask]
@DELL.COM> cc:
Sent by: TechNet Subject: [TN] Connector Contact Finish
<[log in to unmask]>
08/21/2002 02:29 PM
Please respond to
"TechNet E-Mail
Forum."; Please
respond to
Victor_G_Hernandez
Fellow TechNetters,
Requesting for Pro and Cons on the following Connector Surface Plated
finish;
1.) Base material/Ni/Au - Ni is > 250 micro inches and hard Au
30
micro inches
2). Base material/Ni/PdNi/FLASH Au - Gold FLASH over Pd/Ni ( 30
micro inches Min. over Ni 50 micro inches Min.
Os the robustness of this two application the same . I welcome all
comments and publication on process #2.
Victor G. Hernandez
Component/Material Failure Analysis Eng.
PS4-1, Rm. 132
Ofc: 512-725-3471
Pgr: 512-907-0005
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|