thanks Rudy, i think it would be okay to plate 10 micro-inches as along as
i can plate 3-5 microns of Ni underneath (Is Ni-plating bath halide free
also?).
how about other processes such as pre-clean, etc, are there available
halide
free also?
You halides are enemy of semiconductor devices
regards
Rudy Sedlak
<[log in to unmask]> To: [log in to unmask]
Sent by: TechNet cc:
<[log in to unmask]> Subject: Re: [TN] Inquiry
08/16/02 01:38 PM
Please respond to
"TechNet E-Mail
Forum."; Please
respond to
RSedlak
There are non-halide immersion Tins, but they do not deposit thick (>30
microinch) deposits....you need the chloride to drive this engine.
The non-halide immersion Tins will put down say 10 microinches, on a good
day, at temperature.
Rudy Sedlak
RD Chemical Company
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------