Why not put 100u-in of Nickel between the copper and gold? This is typical
industry practice. Gold over copper without solder reflow from the assembly
process is only asking for trouble. After a few years oxidation from the
copper will be very apparent, and depending on the area of contact could
cause failures. The cost for adding the nickel should be minimal.
Be afraid, be very afraid...
Roger Stoops, CID
Trimble Navigation Ltd.
-----Original Message-----
From: Ray Klein [mailto:[log in to unmask]]
Sent: Wednesday, August 14, 2002 8:41 PM
To: [log in to unmask]
Subject: [TN] corrosion on gold flashed PCB's
Guys,
We use 6-8 micro inch of gold flash over copper on our surface layers.
Mostly these areas are covered with solder paste and don't cause a problem.
We are considering using large areas of the board as heat sinks without
solder paste and are concerned with corrosion of the copper underneath this
very thin gold layer. Has anyone tested for or had experience with this?
Ray Klein
JNI
10945 Vista Sorrento Pkwy
San Diego, CA 92130
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|