Daan,
I agree with what Brian said.
I would be more concerned with the adherence of the coating to the plastic.
This can cause problems if the coating delaminates
from the plastic portion of the IC and exposes the leads.
The cleanliness of the ICs will have a direct effect on this issue
(primarily mold release agents, handling, repackaging, and storage).
David A. Douthit
Manager
LoCan LLC
=====================
"d. terstegge" wrote:
> Dear Technetters,
>
> We've just finished our first few boards with Humiseal 1B31 conformal
> coating, applied with a selective spraycoating machine, and we asked the
> customer to inspect the products.
> He commented that some areas on top of the IC's were not covered
> completely, which is required (so he says) because these are plastic
> components which may absorb moisture if left uncovered.
>
> I'm not gonne argue about this with the customer, but still I'm
> interested to hear from you wether the fact that the IC's are plastic is
> indeed a reason to require them to be completely covered with coating.
> As far as my knowledge goes the problem with plastic IC's and moisture
> is limited to the soldering process only, but I may be wrong.....
> Anyone can comment ?
>
> Daan Terstegge
> Unclassified mail
> Personal Website: http://www.smtinfo.net
>
> ---------------------------------------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> ---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|