TECHNET Archives

August 2002

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Thu, 1 Aug 2002 16:45:50 -0400
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="iso-8859-1"
From:
Earl Moon <[log in to unmask]>
Parts/Attachments:
text/plain (112 lines)
Scotch, scotch! Did someone say scotch?


----- Original Message -----
From: <[log in to unmask]>
To: <[log in to unmask]>
Sent: Thursday, August 01, 2002 3:22 PM
Subject: Re: [TN] Solder/Flux Cleaning Methods


> Marshall,
> You ask enough questions to keep me typing for a week.  I would suggest
> that you look in the Technet archives, because this topic has been
> discussed on numerous occasions in the past.  You will find long
> explanations from myself and Brian Ellis that will answer some of your
> questions.  Second, find a copy of J-HDBK-001 and read section 4 (fluxes)
> and section 8 (cleaning).  Brilliantly written stuff.  The handbook is a
> companion to J-STD-001 and has much information on assembly and materials
> choices.  Third, I suggest you get a copy of IPC-TP-1115, which covers
> important considerations if you chose to go no-clean.  After reading
> through those documents, I'd be glad to help.
>
> On your question regarding cleaning with a toothbrush and soapy water:
> what was the brand of scotch he was drinking and was he on his 8th or 9th
> round?
>
> The short answer is that there are no easy answers to your questions and
no
> one can do your homework for you.  Good luck.
>
> Doug Pauls
> Rockwell Collins
>
>
>
>
> Marshall Hopkins <[log in to unmask]>@ipc.org> on 08/01/2002 10:14:28 AM
>
> Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please
respond
>        to Marshall Hopkins <[log in to unmask]>
>
> Sent by:    TechNet <[log in to unmask]>
>
>
> To:    [log in to unmask]
> cc:
>
> Subject:    [TN] Solder/Flux Cleaning Methods
>
>
> I am interested in the most appropriate cleaning method for PCBs after
> soldering. I do not have a bath, but am able to brush or spray alcohol or
> flux-off over the board. I can never get it as clean as when it is
initally
> stuffed and cleaned before returning to me. In military applications,
> especially those that operate in saltwater enviornments, it is very
> important that I can clean the board just in case I have to touch up a
> solder joint or replace a part. Is there a particular solder that makes
the
> job easier such as organic core, rosin core, no-clean, etc...? Also, is
> there a particular type of cleaner that works best with the different
> solder types? I was told that a toothbrush and soapy water could remove
> some flux. Seems like that would be a nice method with readily available
> products. Finally, maybe it is the flux and not the solder that really
> matters. Are there different types of fluxes that are easier to clean than
> others? Any help is greatly appreciated.
>
> --------------------------------------------------------------------------
-------
>
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
> ext.5315
> --------------------------------------------------------------------------
-------
>
> --------------------------------------------------------------------------
-------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
> --------------------------------------------------------------------------
-------

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2