Yep Norman,
caus' it's named bluetape
bye
Ingemar
-----Original Message-----
From: Norman S. Robinson
Sent: den 7 augusti 2002 23:39
To: [log in to unmask]
Subject: Re: [TN] blue mylar
Hi Ingemar.
We used it as a backing film on which to dice up wafers into chips and
after that temperature it made the chips darn difficult to remove for IC assembly.
Depends what Joyce has in mind to use it for.
Cheers . . . Norm
Hi jk,
as it's a PVC it should survive, but will be very soft. We have used Mylar in transformers for decades (Mylar is old stuff). For high T we use Kapton instead.
see: http://www.nitto.com/product/manufacture/spv224-214.htm
http://www.nitto.com/product/manufacture/ip03-2.html
If you need closer data I have friends who know a lot about Mylar.
Why not send DENKA a q?
Ingemar Hernefjord
Ericsson Microwave Systems
-----Original Message-----
From: joyce [mailto:[log in to unmask]]
Sent: den 6 augusti 2002 18:08
To: [log in to unmask]
Subject: [TN] blue mylar
Importance: High
Help, guys!
Does anyone know what is the blue mylar tape (Nitto tape spv 224) maximum
operating temperature? Can it survive for 125 C for extended time (few
hours)? I have difficulty to find the data sheet on line. Many thanks.
Best regards,
jk
< / > < \ > < / > < \ > < / > < \ > < / > < \ >
Norman S. Robinson
E-mail 1: [log in to unmask]
E-mail 2: [log in to unmask]
--------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|