Hi Michael,
It depends a lot on the type of paste you're using, but I believe with
most pastes it shouldn't be a problem to have a couple of hours between
stencilling and component placement. The data sheets sometimes have a
graph for tackiness against time, which gives a fair indication.
It can take up to several days before the reflow properties of the
paste are affected, although for fine-pitch components you wouldn't want
to put a board in the oven where the paste has lost its tackiness.
But again: it depends on the material you're using, so please check
with the manufacturer.
Daan Terstegge
Unclassified mail
Personal Website: http://www.smtinfo.net
>>> [log in to unmask] 07/31/02 06:26am >>>
Hi all,
Has anybody got any idea on how long it takes for paste, that has been
stenciled onto a PCB to start and degradate. Our planning department
is
trying to suggest we use one printer to feed two lines and I have had
little
success in advising otherwise. It would basically mean that pasted
PCB's
would sit for 10-60minutes before placement. I have advised that this
is a
bad idea, but I just need some form of information to back this up.
Has
anyone had any experiance in this??? Any information would be
appreciated,
Cheers
Mike
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV
1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for
additional
information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|