Hi Pat! You will have molten Sn60 solder at a temperature of 1000C! Tin
boils at 2603C and Lead boils at 1750C so you won't start vaporizing the
Sn60 solder alloy until you get near the 1750 C point. I just have to ask -
why the concern of 1000C? Your printed wiring assembly will be quite toasty
and you would have molten solder running on the floor before you reach the
1000C mark!

Dave Hillman
Rockwell Collins
[log in to unmask]




"Diamond, Pat" <[log in to unmask]>@ipc.org> on 07/24/2002 08:38:17 AM

Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond
       to "Diamond, Pat" <[log in to unmask]>

Sent by:    TechNet <[log in to unmask]>


To:    [log in to unmask]
cc:

Subject:    [TN] Overheated solder alloy


Technetters,

this may seem like a crazy question but.....what would happen to 60/40
solder alloy at temperatures of 1000 degrees C?

regards,

Pat Diamond
Weston Aerospace

---------------------------------------------------------------------------------

Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
---------------------------------------------------------------------------------

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2