TECHNET Archives

July 2002

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Transfer-Encoding:
quoted-printable
Sender:
Subject:
From:
Steve Thomas <[log in to unmask]>
Date:
Wed, 31 Jul 2002 09:16:05 -0700
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Steve Thomas <[log in to unmask]>
Parts/Attachments:
text/plain (23 lines)
Greetings...

Our overseas assembler wants us to add a line of silkscreen between pads on bottom-side 0603 R's and C's, 
apparently as a solder dam to reduce bridging in wave solder.  There already is mask between pads, so this seems 
a bit out of the ordinary (we do very little two-sided assembly here but I have never seen bridging on chips). 

Has anyone ever seen this done?  Does this sound like a design band-aid to fix a process problem (talk about the flip side of
a coin!)?  How do you attribute a bridge underneath a glued-on part to wave solder?  I don't have the benefit of a thorough 
knowledge of their process, but I'm speculating they may be printing their glue with a squeegee contaminated with solder paste.  

Your thoughts?

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2