Michael,
We use Garolite (G-10) material for our test bed fixtures. Unfortunately, I
have never done a study to see if can retain a static charge. I believe it
is similar to FR-4 used to make PC boards. It is available in large sheets
from McMaster-Carr.
We drill and place spring loaded contact probes (IDI, QA, Everett Charles)
for our test beds. Works quite well.
Blair Hogg
QA Manager
GAI-Tronics Corporation
-----Original Message-----
From: Michael Bell [mailto:[log in to unmask]]
Sent: Tuesday, July 16, 2002 4:15 PM
To: [log in to unmask]
Subject: [TN] Test/Pin Jig Materials
Hi all,
I am just looking into the best material in which to make the main plate of
a pin bed test jig. I am wanting some insulative plastic, but I am a
little concerned over the static properties of most plastics/acrylics. Does
anyone have any idea on the best type of plastic/acrylic/urethane etc to use
in this application to minimise the static risk, or is there an anti-static
plastic about that I can purchase in large blocks for milling???
Cheers
Mike
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|