you might be able to find an after market adapter. I forwarded your original post to a company qfp-adapter.com and asked them to help out.
When you mentioned the heel hangs off of the end of the pad, did you mean that the heel overhangs the front or back of the pad? If the pad overhangs the front, well, you are in a pickle. But if the heel is the only part of the solder joint that can not be achieved then why not determine the amount of joint that could be maintained to section 12 and then go for a deviation from any heel joint requirements due to an incorrect pad layout.
Kathy
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
<!DOCTYPE HTML PUBLIC "-//W3C//DTD HTML 4.0 Transitional//EN">
<HTML><HEAD>
<META http-equiv=Content-Type content="text/html; charset=iso-8859-1">
<META content="MSHTML 6.00.2715.400" name=GENERATOR></HEAD>
<BODY style="MARGIN-TOP: 2px; FONT: 8pt MS Sans Serif; MARGIN-LEFT: 2px">
<DIV>you might be able to find an after market adapter. I forwarded your
original post to a company qfp-adapter.com and asked them to help out.
</DIV>
<DIV> </DIV>
<DIV>When you mentioned the heel hangs off of the end of the pad, did you mean
that the heel overhangs the front or back of the pad? If the pad overhangs
the front, well, you are in a pickle. But if the heel is the only part of
the solder joint that can not be achieved then why not determine the amount of
joint that could be maintained to section 12 and then go for a deviation from
any heel joint requirements due to an incorrect pad layout. </DIV>
<DIV> </DIV>
<DIV>Kathy </DIV></BODY></HTML>
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|