On 31 Jul 2002 at 16:26, Michael Bell wrote:
> Hi all,
>
> Has anybody got any idea on how long it takes for paste, that has been
> stenciled onto a PCB to start and degradate. Our planning department
> is trying to suggest we use one printer to feed two lines and I have
> had little success in advising otherwise. It would basically mean
> that pasted PCB's would sit for 10-60minutes before placement. I have
> advised that this is a bad idea, but I just need some form of
> information to back this up. Has anyone had any experiance in this???
> Any information would be appreciated,
Maybe it is not totally what you want to hear, but: It depends. I
tried (for low volume stenciling or dispensing, prototyping /manual
p'n'p purposes) many pastes and ended with an Alpha paste RMA390D3K
which can without any problems sit a whole day and is tacky enough
and reflows fine (visually according IPC-A-610) even if itself is
(against all recommendations - I wouldn't do this with customer
stuff) two years outdated and the components have five year old
datecodes.
Regards
Matthias Mansfeld
-----------------------------------------------
Matthias Mansfeld Elektronik
* Printed Circuit Board Design and Assembly
Am Langhoelzl 11, D-85540 Haar, GERMANY
Phone: +49-89-4620 0937, Fax: +49-89-4620 0938
E-Mail: [log in to unmask]
Internet: http://www.mansfeld-elektronik.de
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|