Hi Phil,
Having used Litz wire the past 4 years, I completely understand your brittle
wire situation. We to used a solder pot to tin the wire. I attribute the
brittleness of the wire to the enamel on the individual Litz wire strands.
During the tinning, I think the enamel reflows and the strands become a
single brittle mass.
Maybe you could try using a heat sink around the wire during tinning to stop
heat from running to far up the wire causing the embitterment.
Hope this helps,
Mike Di Giacomo
Process Development Engineer
microHelix Inc.
Portland, Oregon
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Phil Nutting
Sent: Wednesday, July 10, 2002 5:37 AM
To: [log in to unmask]
Subject: [TN] Tinned wire breaking
Good morning,
In many of our designs we use Litz wire. To make a connection with Litz
wire the enamel coating from each strand must be removed. Historically we
have used a small solder pot to tin the ends of the Litz wire. Currently we
have a situation where these tinned wires (about 20 AWG) are breaking when
bent around a turret connection. Initially we thought it was due to the
solder pot having been turned up too high, but I just ran some tests with
the pot at normal temperatures and the wire is still brittle. (Gee, what is
my "standard" temperature.... just measured it at 900°F.... oops, that's a
little high).
What temperature do you folks run small solder pots at? Should I be in the
700-750°F range?
Are there any other thoughts on why the wire is so brittle?
Thanks in advance,
Phil Nutting
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|