Subject: | |
From: | |
Reply To: | TechNet E-Mail Forum. |
Date: | Wed, 10 Jul 2002 08:36:33 -0400 |
Content-Type: | text/plain |
Parts/Attachments: |
|
|
Good morning,
In many of our designs we use Litz wire. To make a connection with Litz wire the enamel coating from each strand must be removed. Historically we have used a small solder pot to tin the ends of the Litz wire. Currently we have a situation where these tinned wires (about 20 AWG) are breaking when bent around a turret connection. Initially we thought it was due to the solder pot having been turned up too high, but I just ran some tests with the pot at normal temperatures and the wire is still brittle. (Gee, what is my "standard" temperature.... just measured it at 900°F.... oops, that's a little high).
What temperature do you folks run small solder pots at? Should I be in the 700-750°F range?
Are there any other thoughts on why the wire is so brittle?
Thanks in advance,
Phil Nutting
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|