Hi Victor,
There is no standardized shear-test for BGAs. The only value such a test has
is to see whether or not the failures occur as interfacial separation [=no
wetting of solder to on of the metallization pads/or weak metallization layer
adhesion], pad/resin adhesion failure [=proof of good solder joint], or
solder joint fracture [=proof of good solder joint]. Numerical values are
useless. Therefore, a test like Sun Microsystems "chisel test" [yes,=chisel
and hammer judiciously applied] is perfectly adequate.
Werner Engelmaier
Engelmaier Associates, L.C.
Electronic Packaging, Interconnection and Reliability Consulting
7 Jasmine Run
Ormond Beach, FL 32174 USA
Phone: 386-437-8747, Fax: 386-437-8737
E-mail: [log in to unmask], Website: www.engelmaier.com
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|