Joyce,
You are way too cool today but, as always, right on. Is that a flaw too?
Sure you use a metal core or metal sandwiched board. You also get the heat
into the core then out of the box using cold walls connected directly to, or
near via heat pipes, the metal plane to conduct heat out of the box.
How many variations on this theme? I used ten oz. Cu a couple of times. CIC,
and related metal cores, both constraining and tailoring, work well.
Lot's to choose from depending on the application and requirement.
MoonMan
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|