Over the years, I have seen a lot of really messed-up solder joints,
especially on coated boards coming back for repair. If a test engineer
can't get his probes to make good contact, the tendency is to grind the
probe into the solder joint until he (or she) either does make contact or
gives up. By that time the solder joints are so mutilated by all the effort
that they have to be touched up with a soldering iron - an unnecessary
thermal excursion that does as much or more harm than good.
Actual recorded data, I don't have - only have this anecdotal stuff and
conclusions about theoretical reliability drawn therefrom.
Peter
Timothy Ground <[log in to unmask]> 17/07/2002 08:20 PM
Sent by: TechNet <[log in to unmask]>
Please respond to "TechNet E-Mail Forum."; Please respond to Timothy Ground
To: [log in to unmask]
cc: (bcc: DUNCAN Peter/Asst Prin Engr/ST Aero/ST Group)
Subject: [TN] ICT points
I have a question about In-Circuit Test for the group....
We have a new customer that has not given us test points in their PWB
design, leaving us few options but to probe components directly or not at
all. Of course, we don't find this acceptable, and want to push back on
the customer. Is anyone aware of any actual data regarding compromised
reliability or other problems that would come from probing parts? Thanks.
Tim
Tim Ground
Quality Engineer
Kimball Electronics Group
ph: 812.634.4552
fax: 812.634.4112
[log in to unmask]
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/html/forum.htm for additional information, or
contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
[This e-mail is confidential and may also be privileged. If you are not the
intended recipient, please delete it and notify us immediately; you should
not copy or use it for any purpose, nor disclose its contents to any other
person. Thank you.]
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|