Linda,
In a nutshell here is what we do. We first start with a good standard solder connection with a short or clinched lead. Then we heat up the joint and add more solder until there is a nice dome over the whole solder joint. If you leave the soldering iron on the solder too long you will get spikes as the solder ages.
There may be specs with quantifying numbers of how high, angle of curve, etc. This is something that I haven't found extensive data/specs to support. It is something that is unique to those of us who are working with higher voltages.
Phil Nutting
-----Original Message-----
From: Linda Langley [mailto:[log in to unmask]]
Sent: Monday, July 15, 2002 8:42 AM
To: [log in to unmask]
Subject: [TN] Ball Solder for High Voltage
Anyone out there know where I can get some information about Ball Solder
Techniques? IPC-610 gives some inspection standards but I would like to
have some type of procedure for making that type of solder joint. Or, point
me in the right direction for finding information.
Thanks
Linda
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|