electrolytic/Inge
-----Original Message-----
From: joyce [mailto:[log in to unmask]]
Sent: den 24 juni 2002 19:00
To: TechNet E-Mail Forum.; Ingemar Hernefjord (EMW)
Subject: RE: [TN] Wire bondable gold
Hi, Inge, could you let me know if you bonded on Ni-P or Ni (electrolytic?).
thanks...jk
>-----Original Message-----
>From: TechNet [mailto:[log in to unmask]]On Behalf Of Ingemar Hernefjord
>(EMW)
>Sent: Monday, June 24, 2002 8:51 AM
>To: [log in to unmask]
>Subject: Re: [TN] Wire bondable gold
>
>
>Steve & Steve,
>we have been wedgebonding directly on heavy nickelplated
>aluminium plates without problem, large mass use to couple
>mechanical waves better than weak materials that swing by. So, I
>think too that it has to do with the gold structure, hardness or
>temperature . First thing we use to do is using hard rubber or
>scalpel blade, just to make sure we don't have some surface
>contamination. Next, check workholder, both for temperature and
>mechanical support. If there is a space between the object and the
>workholder, ultrasonic mismatch can make bonding impossible.
>Another annoying matter is sometimes that the insulator becomes to
>soft, as Steve says, then you may have to try without preheat. I
>assume you have the correct capillary and wire hardness for the job.
>
>Ingemar Hernefjord
>Ericsson Microwave Systems
>
>
>
>-----Original Message-----
>From: Creswick, Steven [mailto:[log in to unmask]]
>Sent: den 24 juni 2002 12:05
>To: [log in to unmask]
>Subject: Re: [TN] Wire bondable gold
>
>
>Steve,
>
>I echo what Joe has already said. This amount of gold should not be a
>problem for gold wire bonding unless the components have not attained
>bonding temperature (on the order of 150C), or something is
>moving/softening
>during bonding.
>
>Even aluminum wire should bond well to this amount of gold - but
>also as Joe
>indicated, the long term reliability may be of some question.
>
>See if the Customer can share a bit more info with you as to the type of
>bonding performed, temperatures, and the type of problems experienced.
>
>Steve Creswick - Gentex
>
>-----Original Message-----
>From: Steve Kelly [mailto:[log in to unmask]]
>Sent: Saturday, June 22, 2002 11:22 AM
>To: [log in to unmask]
>Subject: [TN] Wire bondable gold
>
>
>We made some flex circuits for a customer and wound up putting too
>much gold
>on - approx. 75 microinches. The nickel is averaging 153. The gold
>meets all
>the purity specs. Under the wire bond area is a large heat sink.
>My customer
>is having difficulties wire bonding. Is too much gold a problem or can the
>heat sink cause issues. Regards Steve Kelly
>--------------------------
>Sent from my BlackBerry Wireless Handheld (www.BlackBerry.net)
>
>-------------------------------------------------------------------
>---------
>-----
>Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt delivery of Technet send e-mail to
>[log in to unmask]: SET
>Technet NOMAIL
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
>information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
>ext.5315
>-------------------------------------------------------------------
>---------
>-----
>
>-------------------------------------------------------------------
>--------------
>Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
>information, or contact Keach Sasamori at [log in to unmask] or
>847-509-9700 ext.5315
>-------------------------------------------------------------------
>--------------
>
>-------------------------------------------------------------------
>--------------
>Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
>information, or contact Keach Sasamori at [log in to unmask] or
>847-509-9700 ext.5315
>-------------------------------------------------------------------
>--------------
>
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|