If overall thickness is above .100 I might increase time to 4 hrs, but
otherwise the recommended bake cycle looks great.
Ron
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Rick Thompson
Sent: Tuesday, June 04, 2002 6:50 PM
To: [log in to unmask]
Subject: [TN] Rigid-Flex Bake Requirements??
We're assembling a fairly complex rigid-flex PCB (10 layer, sub-4mil
line/space, polyimide/FR4 sandwich) and have had some issues with
bake-out to remove moisture. The boards we received were individually
sealed with dessicant pack and humidity indicator card in each. Our
assumption was that they did not need baking since they were sealed and
had been fabricated only a couple of days prior. The board vendor is
telling us they need 2 hours at 250 F bakeout, regardless of packaging.
My question is this: Can anyone offer any guideline, insight, etc into
the baking that may be required for this type of rigid-flex PCB? Are
there any industry standards that may cover this?
Thanks in advance,
Rick Thompson
Ventura Electronics Assembly
2655 Park Center Dr.
Simi Valley, CA 93065
+1 (805) 584-9858 x-304 voice
+1 (805) 584-1529 fax
[log in to unmask]
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|