yap, polyimide board should be OK and you need high temp solder (very high
compare to the eutectic Sn/Pb).
good luck.
jk
>-----Original Message-----
>From: TechNet [mailto:[log in to unmask]]On Behalf Of Eddie Rocha
>Sent: Wednesday, June 26, 2002 12:37 PM
>To: [log in to unmask]
>Subject: [TN] High operating temperature
>
>
>Can someone recommend a laminate for product that will, at
>times see operating temperatures of 205C for 4 hours. Also
>would this require a different solder? Will solder reflow?
>Any comments?
>thanks,
>
>-------------------------------------------------------------------
>--------------
>Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
>information, or contact Keach Sasamori at [log in to unmask] or
>847-509-9700 ext.5315
>-------------------------------------------------------------------
>--------------
>
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|