Carl: The elastomeric to tin/lead(HASL)contact switch will work fine for
your prototype.
Over time the tin/lead forms an oxide layer that raises the contact
resistance resulting in an intermittent connection that can gradually
deteriorate to an open. However at normal conditions it can take years to
form a thick enough oxide layer to cause problems.
If you can live with something in a 20-30 ohm/sq contact resistance on the
board you may want to consider a carbon polymer thick film (PTF). It will
retain the same contact resistance over time. Your quick turn shop may
offers this. Also if this is applicable to the finished design it might be
cheaper than gold; depending on the gold type, thickness and process.
Over the years we have used all three; tin/lead, PTF and gold for a variety
of applications with elastomeric switches.
Regards
Michael Barmuta
Staff Engineer
Fluke Corp
Everett WA
425-446-6076
-----Original Message-----
From: Carl VanWormer [mailto:[log in to unmask]]
Sent: Wednesday, June 19, 2002 1:56 PM
To: [log in to unmask]
Subject: [TN] Not gold fingers on prototype conductive elastomer switch
I am making a prototype handheld unit that uses a conductive elastomeric
button to short out an interdigitated pattern as a switch (just like in your
TV remote). The quick turn prototype house I will be using does not offer
gold plating in their fast/cheap process, so I plan to live with the HASL
finish for this switch. Have any of you guys tried this before? How short
will the useful life be, when compared to the standard elastomer on gold?
Thanks,
Carl
Carl Van Wormer
Cipher Systems
1815 NW 169th Place, Suite 5010
Beaverton, OR 97006
Phone (503)-617-7447 Fax (503)-617-6550
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|