Dear Ingemar,
The materials that can be used to meet high operating temperatures for PCBs
can be any of BT Epoxy or Poyimide.
Some of the processing parameters wil differ from Normal FR-4 material
requirements.
Regards,
M A Ranganath
GM - Technical & Quality
Sanmar Micropack Limited
Plot No.16, Jigani Industrial Area,
Bangalore - 562 106. INDIA
Phone: 91 - 80 - 7825223/224/226/389
Fax : 91 - 80 - 7825225
Email : [log in to unmask]
"Ingemar Hernefjord (EMW)"
<[log in to unmask] To: [log in to unmask]
ICSSON.SE> cc:
Sent by: TechNet Subject: Re: [TN] High operating temperature
<[log in to unmask]>
06/27/02 12:12 PM
Please respond to "TechNet
E-Mail Forum."; Please
respond to "Ingemar
Hernefjord (EMW)"
Hi Eddie,
we made some odd circuits for missiles many years ago, LTCC substrates will
do the job and also if you can use gold/tin solder. But we had rather few
components, most of them ceramics and semis. Just an idea, don't know what
kind of equipment you are planning.
Ingemar
-----Original Message-----
From: Eddie Rocha [mailto:[log in to unmask]]
Sent: den 26 juni 2002 18:37
To: [log in to unmask]
Subject: [TN] High operating temperature
Can someone recommend a laminate for product that will, at
times see operating temperatures of 205C for 4 hours. Also
would this require a different solder? Will solder reflow?
Any comments?
thanks,
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]:
SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]:
SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
---------------------------------------------------------------------------------
* * * * * * * * * * * * * * * * * * * * * * * * * * * * * *
The information contained in this message is legally privileged and
confidential information intended only for the use of the addressed
individual or entity indicated in this message (or responsible for
delivery of the message to such person). It must not be read, copied,
disclosed, distributed or used by any person other than the addressee.
Unauthorised use, disclosure or copying is strictly prohibited and may be
unlawful.
Opinions, conclusions and other information on this message that do not
relate to the official business of any of the constituent companies of
the SANMAR GROUP shall be understood as neither given nor endorsed by
the Group.
If you have received this message in error, you should destroy this
message and kindly notify the sender by e-mail.
Thank you.
* * * * * * * * * * * * * * * * * * * * * * * * * * * * * *
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|