Hello Peter, a supported hole is a plated through hole and an unsupported
hole does not have any plating in the hole, mostly found on single sided
board or from secondary drilling operations.
Hope this helps,
Regards,
Leo Lambert
EPTAC Corp
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Peter Lee
Sent: Tuesday, June 25, 2002 3:22 PM
To: [log in to unmask]
Subject: [TN] Definition of Suported/ unsupported hole
Technet,
Can anyone explain the difference between a supported
and unsupported hole on PCB?
I am reading a section on IPC-A-600 RevF and section
2.10.3/4 specify difference acceptance criteria
according to the hole type.
Rgds,
Peter
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|